FISCHERSCOPE ST200

The FISCHERSCOPE® ST200 is Fischer's first automatic scratch-test system for characterizing hard material layers. Easily check the adhesion and cohesive strength of layers ≥1 μm thick. The instrument is ideal for use in development, quality assurance, incoming goods control and production monitoring.

FISCHERSCOPE ST200, st200, Scratch Tester, adhesion strength testing, cohesive strength testing
FISCHERSCOPE ST200 Scratch Tester is used for automated testing of the adhesion and cohesive strength of hard material layers.

Features

  • Diverse measurement modes with progressive, constant or incrementally increasing test force
  • Measure according to the following norms: ASTM C1624, ISO 20502 and DIN EN 1071-3
  • Force control for measuring on curved surfaces
  • Three analysis methods: optical microscopy, friction force, acoustic emission
  • Intuitive user interface – only a brief familiarization is required to use the instrument
  • Fast measurements with motorized XY-stage and Z-axis
  • Easy creation of test reports

Applications

  • Testing how well thin coatings adhere to their substrates
  • Automated measurements with high sample throughput
  • Hard material coatings (PVD, CVD)
  • Components for vehicle engines and drivetrains
  • Electroplated layers (decorative, functional)
  • Characterization of hard anodized coatings
  • Special materials for medical technology
  • Electronic components, plugs, etc.
  • Layers applied via plasma treatment

Your contact to FISCHER

Fischer Instrumentation (GB) Ltd
Lymington/Hampshire/United Kingdom

Contact directly
Phone: +44 (0) 1590 684100
E-Mail: mail@fischergb.co.uk
Online contact form

Information

Downloads